Description
Liquid viscosity | 200-350MPa·s |
Liquid density | 1.15-1.36g/cm3 |
Flexural modulus | 1.882-2.385 MPa |
Bending strength | 60-72MPa |
Heat distortion temperature | 130℃ |
Thermal expansion coefficient | 97*E-6 |
Volume shrinkage | 3.26-3.75% |
Linear shrinkage | 0.9-1.25% |
Tensile St rength | 42-62Mpa |
Tensile modulus | 1.86-2.645MPa |
Tensile strain at break | 11%-21% |
Shore hardness | 82-88D |
Glass transition temperature | 125℃ |
Density after curing | 1.18-1.42g/cm3 |
Notched impact strength | 60-80j/m |
Optimal storage temperature | 20℃~25℃ |
Curing wavelength | 405nm |